彩鋼夾芯板有漆色脫落以及爆漆屬于正常的現象,但這不僅會影響不銹鋼玻鎂板的應用,還會繼續影響內飾的美觀大方,那么造成彩鋼夾芯板漆色脫落以及爆漆的原因是什么?
It is normal for color steel sandwich board to have paint color fall off and paint explosion, but this will not only affect the application of stainless steel glass magnesium plate, but also continue to affect the beautiful and generous interior, so what is the cause of color steel sandwich board paint color fall off and paint explosion?
造成彩鋼夾芯板漆色脫落的原因
Cause color steel sandwich plate paint color off
建筑幕墻路基不干凈,或水不足。密封圈過厚或放水太多。不銹鋼瓦反面塵土未消除或水未充足浸濕。不銹鋼玻鎂板反面的污垢在鋪裝時沒有清洗整潔,水跡太多,導致迎合不合理。
Building curtain wall roadbed is not clean, or water is insufficient. Seal ring too thick or too much water. The dust on the opposite side of the stainless steel tile is not eliminated or the water is not adequately soaked. The dirt on the opposite side of the stainless steel glass magnesium plate is not cleaned and tidy when paving, and there are too many water marks, leading to unreasonable catering.
因為強力膠相對密度不一致,初凝期后強力膠地基沉降,導致墻面空鼓、松脫。與強力膠的膨脹系數不一樣,大容量不銹鋼玻鎂板鋪裝后存有溫度差內應力,周期性溫度差震蕩會導致粘接抗壓強度。
Because the relative density of superglue is not consistent, the foundation of superglue settles after the initial setting stage, resulting in hollow drum and loose wall. Different from the expansion coefficient of super glue, the large capacity stainless steel glass magnesium plate has internal stress of temperature difference after installation, and periodic temperature difference shock will lead to the bonding compressive strength.
造成彩鋼夾芯板漆色爆漆的原因
Cause color steel sandwich board paint color explosion reason
有時伴隨著溫度持續減少,許多地域牽涉到各種類型的彩鋼夾芯板都出現了爆漆狀況。彩鋼夾芯板爆漆天氣確實有關系嗎?實際上這不是所有緣故。
Sometimes accompanied by the continuous reduction of temperature, many regions involved in various types of color steel sandwich plate have appeared paint explosion. Does color steel sandwich board paint weather really matter? Actually, that's not all.
彩鋼夾芯板生產工藝流程中規定,彩鋼夾芯板的溫度必須每兩小時查驗一次,假如工作員沒有準時追蹤把握溫度,特別是在冬天,溫度在2鐘頭內改變比較大,較終究會造成涂顏色時間較長,造成爆漆。
Color steel sandwich plate production process stipulated that the temperature of color steel sandwich plate must be checked every two hours, if the staff did not track the temperature on time, especially in winter, the temperature changes in 2 hours is relatively large, will eventually cause a longer color coating time, resulting in paint explosion.
在彩鋼夾芯板生產過程中,出入口檢測鏡和滾桶上的灰塵會立即營銷推廣色漿的上色實際效果,一開始不容易非常顯著,在太陽下能呈現。
In the production process of color steel sandwich plate, the dust on the entrance and exit inspection mirror and barrel will immediately promote the actual effect of color paste coloring, at the beginning is not easy to be very significant, can be presented in the sun.
彩鋼夾芯板具備質輕,高韌性,隔熱保溫,美觀大方經久耐用等彩鋼板勢,是工程建筑與裝修融為一體的高級建設工程。所以想更好的使用它就要多了解它,那么就來這里www.www032378.com咨詢吧。
Color steel sandwich plate has light weight, high toughness, heat insulation, beautiful and durable color steel plate potential, is a senior construction project of engineering construction and decoration. So if you want to better use it to know more about it, then come here to www.www032378.com for advice.